logo
Dom ProduktyNieniszczący sprzęt testujący

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment

Najlepsze produkty
Orzecznictwo
Chiny HUATEC  GROUP  CORPORATION Certyfikaty
Chiny HUATEC  GROUP  CORPORATION Certyfikaty
Opinie klientów
szeroka gama produktów NDT, możemy uzyskać wszystko w grupie huatec. Wolimy kupować od nich. Rudolf Shteinman Rosja

—— Rudolf Shteinman

Podoba mi się serwis, bardzo szybka reakcja, profesjonalna praca. Aret Turcja

—— Aret Kaya

Tester twardości huatec, bardzo dobrej jakości, jesteśmy bardzo zadowoleni z przenośnego testera twardości RHL-50. Kumaren Govender Sotuth Africa

—— Kumaren Govender

Im Online Czat teraz

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment
HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment

Duży Obraz :  HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment

Szczegóły Produktu:
Miejsce pochodzenia: Chiny
Nazwa handlowa: HUATEC
Orzecznictwo: CE
Numer modelu: HCDX-D
Zapłata:
Minimalne zamówienie: 1 szt
Czas dostawy: 7-10 dni roboczych po otrzymaniu płatności
Zasady płatności: T/T, PayPal
Możliwość Supply: 10 zestawów/miesiąc

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment

Opis
Zasilanie: AC 220 V ± 10% 50 Hz 5 A Wyjście: AC 38V 10A
Prędkość kontroli: ≥6 m/min Wzrost temperatury sondy: ≤60 ℃
czas magnesowania: ≤3 sekundy czas przerwy: ≥5 sekund
Podkreślić:

composite magnetic particle flaw detector

,

rotating magnetic field weld crack detector

,

NDT testing equipment with standard D probe

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment


Introduction:

HCDX-D composite magnetic powder flaw detector adopts silicon controlled contactless switch, with low noise, strong magnetic force, long service life and simple operation, suitable for field and laboratory use. The instrument adopts combined configuration, and users can choose probe freely according to their needs. Type A, D, E, O probe can be configured according to user requirements. Especially, type E probe is a crossed yoke probe, which can produce a rotating magnetic field, so as to conduct a comprehensive inspection on a variety of straight seam, girth weld, butt weld, geometric shape of plane and curved surface.

 

All optional probes parameters:

D type probe

Lifting force: AC≥5Kg DC≥18Kg (no joints)

Pole distance: 50-200mm (adjustable)

Operating current: ≥8A

Working voltage: AC=38V, DC=9V

Weight: 2.5 Kg

Atype probe

Lifting force: AC≥ 4.5kg DC≥18Kg

Pole distance: 20-160mm (adjustable)

Working voltage: AC=38V, DC=9V

Weight: 2.0 Kg

Otype probe

Central magnetic intensity: 180Oe

Working voltage: AC=38V

Inside diameter: 150 mm

Weight: 2.5 Kg

Etype probe

Lifting force: ≥12Kg

Distance: 110 mm

Operating current: ≥7A

Inspection speed: 6 m/min

Working voltage: 38 v left, 2

Weight: 3.0 Kg

 

Application:

Mainly used to detect surface and near surface cracks of ferromagnetic workpiece.

Boiler pressure vessel, steel structure, forgings, castings, welding parts, machined parts, etc.

 

The standard probes introduction for model HCDX-D:

 Type D probe (electromagnetic yoke probe): equipped with movable joints, can magnetize and detect the surface workpiece.

 

Technical parameters:

Power supply: AC 220V ± 10% 50HZ 5A

Output: AC 38V 10A

Type A.D.E.O probes are optional and available

Inspection speed: ≥6 m/min

Temperature rise of probe: ≤60℃

Working beat: it is recommended to work for a long period of continuous operation: magnetizing time ≤3 seconds, gap time ≥5 seconds

Weight: about 6.5Kg (main unit)

Standard delivery:

 

Host HCDX-D    1

Type D yoke probe 1

The power line    1

The probe line    1

Standard specimen 1

Operation manual  1

Certificate        1

 

Optional accessories:

Type A probe

O the probe

E probe

Dead weight

Test specimen

UV light

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment 0

HCDX-D Composite Magnetic Particle Flaw Detector Rotating Magnetic Field Standard D Probe Weld Crack NDT Testing Equipment 1

Szczegóły kontaktu
HUATEC GROUP CORPORATION

Osoba kontaktowa: Ms. Shifen Yuan

Tel: 8610 82921131,8618610328618

Faks: 86-10-82916893

Wyślij zapytanie bezpośrednio do nas (0 / 3000)

Inne produkty